Apple Mug #2
 
© Whistle Tree Pottery - Ellijay, GA 2015

Apple Mug #2


GA_Clayman67
 Share


Same glaze combo on the embellishment. Body glazes: Amaco Ancient Jasper (4 coats) and rim dipped into Coyote Red/Gold and fired to Cone 6.

 

Clay is Laguna BMix5.

Copyright

© Whistle Tree Pottery - Ellijay, GA 2015
From the album:

Glaze Combinations

  • 3 images
  • 0 comments
  • 1 image comment

Photo Information for Apple Mug #2

 Share


Recommended Comments

There are no comments to display.

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.