© Whistle Tree Pottery - Ellijay, GA 2015


Mug for a local apple merchant. The body glaze is Coyote Red/Gold with a small accent of Gun Metal Green on the rim. Best results are achieved by leaving the upper 1/4-1/2" unglazed and then dipping into the green.

The apple embellishment is hand-painted: Mayco Caramel (Cone 05) - Coyote Really Red and whatever green I'm in the mood for!

 

Clay is Laguna BMix5

Copyright

© Whistle Tree Pottery - Ellijay, GA 2015
From the album:

Glaze Combinations

  • 3 images
  • 0 comments
  • 1 image comment

Photo Information for Apple Mug #1


Recommended Comments

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.