platter with peaches
touching up color where too thin or where it disappeared in the firing. refired to cone 6 in a cool spot to avoid cracking.
cannot get the final glazed pot to post here. computer threw up its hands and screamed ENOUGH when i tried. i had only been trying for several hours. the whole thing froze up and nothing would work for over 25 minutes. it is now 12:58 am. good night all. tried again next day. got it to post in only an hour or so of fighting. final peaches is the name it is under.