Mountain Meg Posted May 27, 2015 Report Share Posted May 27, 2015 Our first cone 10 firing in our West Coast kiln was impressive and we felt very encouraged. We did notice that the kiln door had a new almost glazed like surface in some places....What would have possibly caused this? I appreciate any comments or thoughts. Thanks, Mountain Meg Link to comment Share on other sites More sharing options...
Mark C. Posted May 28, 2015 Report Share Posted May 28, 2015 Kiln finially got dried out good and my guess was all the mositure and cements and binders got hot and the fumes got moving. The soft brick seal at the door can always get discolored. Was the door cranked down tight as its should be. How was the rest of fire (pots turn out and was temp even?) Mark Link to comment Share on other sites More sharing options...