I was just throwing a few mugs with rather specific final dimensions in mind and realized that what I thought to be true may not be. Is clay shrinkage uniform in all directions? For example, if I have a freshly thrown cylinder which stands 6" tall and has a diameter of 4" will the final dimensions be 5.28 by 3.52" after the glaze firing?

#2 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,828 posts
  • LocationGrayslake, IL

Posted 07 May 2013 - 12:55 PM

Yes, the shrinkage is in all directions. I suppose it is posible that one direction could shrink a hair more or less than another depending on the orientation of the clay particles, but that's most likely to happen in slabs. For the sake of calculating the final size, it's all the same.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com


#3 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,070 posts
  • LocationRaleigh, NC

Posted 07 May 2013 - 01:47 PM

Those numbers apply if you know your thrown clay pieces shrink by that %. Have you measured or are you going by the numbers reported on the clay site? I only mention this since you said your measurements are important to the finished work. If it is, being off by even a 1/16" could be a major pain ... if you were thinking of adding a travel lid for example.

Chris Campbell

Contemporary Fine Colored Porcelain
www.ccpottery.com

 

TRY ... FAIL ... LEARN ... REPEAT

" ... If a sufficient number of people are different, no one has to be normal"
Fredrick Bachman


#4 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,828 posts
  • LocationGrayslake, IL

Posted 07 May 2013 - 01:54 PM

I always tell customers I won't be any more exact than 1/4" in any direction, 1/2" on larger pieces.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com


#5 OffCenter

OffCenter

    Advanced Member

  • Members
  • PipPipPip
  • 1,372 posts

Posted 07 May 2013 - 02:23 PM

I always tell customers I won't be any more exact than 1/4" in any direction, 1/2" on larger pieces.


Hopefully that doesn't apply for your lids.

Jim
E pur si muove.

"But it does move," said Galileo under his breath.

#6 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,828 posts
  • LocationGrayslake, IL

Posted 07 May 2013 - 03:30 PM


I always tell customers I won't be any more exact than 1/4" in any direction, 1/2" on larger pieces.


Hopefully that doesn't apply for your lids.

Jim


No, because you don't have to calculate shrinkage with lids! It only applies to when they say they want a piece of a certain size.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com





0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users