i'm looking for a tomato red ^6 glaze that I can buy. I don't have the time right now to be mixing one up. I know Seattle Pottery Supply offers one, has anyone used it. Looking for other source and would appreciate any help I can get.

Thanks,
Bob

#2 weeble

weeble

    Advanced Member

  • Members
  • PipPipPip
  • 121 posts
  • LocationOregon Coast

Posted 30 April 2013 - 02:26 AM

Mayco Stroke and Coat Hot Tamale is a nice red without breaking the bank, its a tiny bit more toward the purple side than the orange side, but still RED, its our go-to red at the studio. Just not a huge number of choices out there for red at cone 5-6
Maryjane Carlson

Whistling Fish Pottery

#3 deborah.

deborah.

    Newbie

  • Members
  • Pip
  • 7 posts
  • LocationBlacksburg, VA

Posted 30 April 2013 - 08:32 AM

We use a few glazes by Standard at my community studio including both their bright red and dark red (firing to cone 6). They're #1194 and #1210. I have plenty of experience with both. Neither appear to run, pinhole, craze, or any other glaze flaws. They're pretty happy, stable glazes which is why we continue to use them instead of mixing our own red. Here's the website for them: Standard cone 5/6 glazes

Best of luck,
Deborah

#4 Venicemud

Venicemud

    Advanced Member

  • Members
  • PipPipPip
  • 83 posts

Posted 30 April 2013 - 02:40 PM

i'm looking for a tomato red ^6 glaze that I can buy. I don't have the time right now to be mixing one up. I know Seattle Pottery Supply offers one, has anyone used it. Looking for other source and would appreciate any help I can get.

Thanks,
Bob



Coyote Clay and Color has a couple of reds with their Really Red probably being the most in your face red. I seem to be frequently recommending Coyote glazes, its a little embarrassing, honest I have no financial connection to the company - just a satisfied customer, satisfied with both their glazes and the telephone help I've received when I had questions.

Joan Klotz (Venicemud)