a couple of questions on my first re-fire


  • Please log in to reply
5 replies to this topic

#1 Jime

Jime

    Member

  • Members
  • PipPip
  • 20 posts

Posted 20 April 2013 - 05:40 PM

Hi all
last night was my first ever glaze firing, and I came in a little under temp.
Tonight I'm going to give it another shot and I have a couple of questions.

How fast can I ramp up the temperature? do I just start it on high, or go through medium and low first?
I'm going to switch out the witness cone for a new one, should I also change out the kiln-sitter cone?

Since this was my first glaze firing, I had a LOT of glaze tests in there. do you think that re-firing is going to give me a good idea of what the glazes will look like in the future, or should I assume that the tests won't be a good representation?

some technical details: I'm using commercial clay and glazes, using an electric Cress 23 kiln (small studio size). I bisqued to 04, and I was trying to fire to cone 6. my witness cone began to bend, but is still mostly straight, so I estimate that it got to cone 5.

last night's firing was 2 hours on low, 2.5 on medium, and it took 5 hours on HIGH to get to cone 5 (total firing was 10 hours). That seems long to me, I would have expected it to reach temperature a bit faster. does that sound normal to you?
thanks for all your help, this is pretty exciting!!

#2 gypsy

gypsy

    Advanced Member

  • Members
  • PipPipPip
  • 89 posts
  • LocationJames Creek, Pa

Posted 20 April 2013 - 06:14 PM

Hi all
last night was my first ever glaze firing, and I came in a little under temp.
Tonight I'm going to give it another shot and I have a couple of questions.

How fast can I ramp up the temperature? do I just start it on high, or go through medium and low first?
I'm going to switch out the witness cone for a new one, should I also change out the kiln-sitter cone?

Since this was my first glaze firing, I had a LOT of glaze tests in there. do you think that re-firing is going to give me a good idea of what the glazes will look like in the future, or should I assume that the tests won't be a good representation?

some technical details: I'm using commercial clay and glazes, using an electric Cress 23 kiln (small studio size). I bisqued to 04, and I was trying to fire to cone 6. my witness cone began to bend, but is still mostly straight, so I estimate that it got to cone 5.

last night's firing was 2 hours on low, 2.5 on medium, and it took 5 hours to get to cone 5. That seems long to me, I would have expected it to reach temperature a bit faster. does that sound normal to you?






thanks for all your help, this is pretty exciting!!


It is exciting isn't it? I used to candle then go to medium then high. Now I candle and go straight to high...it works for me.. Good luck on your refire.



#3 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,054 posts
  • LocationRaleigh, NC

Posted 20 April 2013 - 10:22 PM

You are correct. Your results will not be 100% representative of what a single firing would be ... but they might be close enough / might not.

My Cone 5-6 firings take about 6 - 8 hours so that seems OK. Good Luck!

Chris Campbell

Contemporary Fine Colored Porcelain
www.ccpottery.com

 

TRY ... FAIL ... LEARN ... REPEAT

" ... If a sufficient number of people are different, no one has to be normal"
Fredrick Bachman


#4 Marcia Selsor

Marcia Selsor

    Professor Emerita, MSU-Billings

  • Members
  • PipPipPip
  • 6,117 posts
  • LocationRed Lodge, Montana

Posted 20 April 2013 - 10:53 PM

my ^6 firing are like Chris's... 6 to 8 hours. If your are refining porcelain I would not start on high. 'D be worried about shocking the dense body.
marcia
Marcia Selsor, Professor Emerita,Montana State University-Billings
[http://www.marciaselsorstudio.com

#5 Jime

Jime

    Member

  • Members
  • PipPip
  • 20 posts

Posted 20 April 2013 - 11:12 PM

thanks for the help!
I've got it up and running. New cone and bar, and crossing my fingers for great success. I set it for a "fast firing", and I'm keeping notes on how the dial is moving. It did about 1 hour on low, and 1 hour on medium, just now getting to high... hope it's not too fast!

#6 High Bridge Pottery

High Bridge Pottery

    Joel Edmondson

  • Members
  • PipPipPip
  • 1,781 posts
  • LocationNewcastle Upon Tyne. England

Posted 21 April 2013 - 06:58 AM

I do not know much about firing as I have only done it 10ish times. My firing schedule that got the best results was, 1 hour to 300 centigrade then full whack all the way to 1240 centigrade with a 20 min hold. I have no idea if this is the best but it has given me the best results. Maybe I should take it slower to start. Not sure on the time that it takes from 300 to 1240 but probably 4-6 hours.

Stoneware 'buff', electric kiln, digital controller, too much enthusiasm Posted Image

Community Challenge #8     :o  http://community.cer...ty-challenge-8/

Submit your community challenge ideas - http://community.cer...hallenge-ideas/

 


youtube-logo-50x50.png facebook-logo-50.png instahack.png?1

 





0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users