I am new to ceramics and have started working with cone 10 crystal glazes. I am trying to get red under the crystal glaze. I have tried adding copper oxide to the glaze firing it than putting it through reduction at 1700 F for 15 to bring out the red. It has not worked, I sometimes get a little pink but mostly tan. Should I try a red slip and where can I get a formula for it?

Share this post


Link to post
Share on other sites
Pompots    4

I am new to ceramics and have started working with cone 10 crystal glazes. I am trying to get red under the crystal glaze. I have tried adding copper oxide to the glaze firing it than putting it through reduction at 1700 F for 15 to bring out the red. It has not worked, I sometimes get a little pink but mostly tan. Should I try a red slip and where can I get a formula for it?

 

 

A good slip for greenware, 1000 g. of your clay (dried, pulverized), 700g water, 250g Bright Red (inclusion). I really don't know how this would react with the crystal glaze but for sure is a very nice red slip.

Share this post


Link to post
Share on other sites
perkolator    53

i know some folks who have had great success using Duncan "Really Red" at ^10. try it under, on top of, or inside your glaze. only problem i have with it is you get a "crayola" red from the mason stain as opposed to a true copper red. you could add it to any slip recipe if you wanted to color it that way as well. it's all about experimentation!

Share this post


Link to post
Share on other sites
Iforgot    2

Try using one of the really bright red stroke n' coat Mayco underglazes. I have had luck with them at ^10.

 

 

 

Good Luck!

 

Darrel

Share this post


Link to post
Share on other sites
neilestrick    1,381

Copper reds are very specific, touchy formulas that have to be fired just right. Just adding copper to a glaze will most likely not give you a strong red. I would start by comparing some copper red formulas to your glaze recipe to get an idea of what's needed.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×