Hello out there...

I am putting a few pieces in a friend's wood kiln and am looking for suggestions for some glazes (and recipes) that might result in some interesting surfaces. I already use a lot of ash glazes and of course will try a shino. Just wondering if anyone would like to share?? Thanks for your time.

April

Share this post


Link to post
Share on other sites

John Britt's book, The Complete Guide to High Fire Glazes, has some wood-kiln glaze and flashing slip recipes. You might want to start there. Also, check his website and the North Carolina Clay Club blog -- John lists glaze recipes regularly.

Share this post


Link to post
Share on other sites

Hello out there...

I am putting a few pieces in a friend's wood kiln and am looking for suggestions for some glazes (and recipes) that might result in some interesting surfaces. I already use a lot of ash glazes and of course will try a shino. Just wondering if anyone would like to share?? Thanks for your time.

April

 

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×

Important Information

By using this site, you agree to our Terms of Use.