Duncan Kiln 1029 -strange material lid and floor

Recommended Posts

HeatherT    0

Hello,

 

I just bought a Duncan 1029-2. The bricks seem to be in good shape other than the lid and the floor. They seem to be made of some other material than the usual brick used in kilns and I have never seen anything like it. It seems to be disintegrating and looks similar to a fiber blanket material. Does anyone know what it is? Does anyone know if replacing the lid and the floor with regular kiln brick will work?

 

Thank you for your help!

Heather

Share this post


Link to post
Share on other sites
Mark C.    1,797

A photo would really help in this.

Without one my guess and its a wild one at best is ceramic fiber board-never heard of this in a electric kiln but maybe someone thought it would work. This board is like fiber but a tad harder and feels more like cardboard. Are there seems??

Mark

Share this post


Link to post
Share on other sites
HeatherT    0

A photo would really help in this.

Without one my guess and its a wild one at best is ceramic fiber board-never heard of this in a electric kiln but maybe someone thought it would work. This board is like fiber but a tad harder and feels more like cardboard. Are there seems??

Mark

 

 

 

Here are some photos. It does not appear to have a seem. I am assuming I should replace the lid and bottom with normal kiln bricks.

 

Thanks for replying so quickly to both who responded :)

post-17713-13526743449_thumb.jpg

post-17713-135267435415_thumb.jpg

post-17713-135267436685_thumb.jpg

post-17713-135267437459_thumb.jpg

post-17713-13526743449_thumb.jpg

post-17713-135267435415_thumb.jpg

post-17713-135267436685_thumb.jpg

post-17713-135267437459_thumb.jpg

Share this post


Link to post
Share on other sites
Mark C.    1,797

That is ceramic fiber-do not breath the fibers-looks like your lid had a layer glued to it and the floor looks cracked and they put down a layer of fiber-you will need to remove fiber and replace bricks-the lid looks like it has a huge fallout problem onto stuff.You can also just but a new lid and floor as well.

Mark

Share this post


Link to post
Share on other sites
HeatherT    0

That is ceramic fiber-do not breath the fibers-looks like your lid had a layer glued to it and the floor looks cracked and they put down a layer of fiber-you will need to remove fiber and replace bricks-the lid looks like it has a huge fallout problem onto stuff.You can also just but a new lid and floor as well.

Mark

 

 

Ok thank you so much for your help!

Share this post


Link to post
Share on other sites
neilestrick    1,379

I've replaced this type of floor and lid on several Duncan kilns with a typical brick floor/lid. These fiber modules were terribly weak and crumbly.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×