I wonder if anyone can shed some light on this. I found an old glaze book with some great recipes I remember in it. There were some that do not fit the glaze formula adding up to 100% and the additions normally take it over or are in addition to 100%. The two recipes below are examples of what I mean. They are more like a cake recipe made up of various ingredients in a random fashion, one formula adding up to 112% without additions and the other only 94%. The percentages were not with the recipes, I calculated them because the formula did not look correct.

 

Is this way of mixing glazes a correct way or is there a calculation you are supposed to use to convert the glazes so that they fit the 100% rule?

 

Thanks in advance for any insight you can provide.

 

Glaze 1

 

Chemical % Grams

Kona F-4 54% 1620

Silica 29% 870

EPK 8% 240

Magnesium Carb 8% 240

Bone Ash 13% 390

Sub-Total 112% 3660

Plus

RIO 8% 240

Bentonite 2% 60

Totals 122% 3960

 

Glaze #2

Custer Feldspar 45% 1350

Whiting 13% 390

Silica 25% 750

EPK 11% 330

Sub-Total 94% 2820

RIO 8% 240

Bentonite 2% 60

Totals 104% 3120

 

Sorry for the way this is formatted - I tried 5 different ways and it always turns out a mess. Hopefully you will be able to decipher it.

Share this post


Link to post
Share on other sites
Mark C.    1,807

Some of my old but still used glazes formulas do not add up to 100%

Thats just the way it is and they work great.

Mark

Share this post


Link to post
Share on other sites
JBaymore    1,432

To convert a glaze recipe in any amount format to a glaze raw materials percentage relationship, add up the total of all the ingredients in the original recipe. Then divide each single ingredient item's original number by that overall total number. It will now be set up in a percentage format.

 

The usual "convention" in the filed is that the "main ingredients" add up to 100%, and then things like opacifiers, colorants, a small addition of benonite , and so on are above and beyond the total of the "base glaze". But this in no way is mandatory nor does it affect anything.

 

For those of us who also use molecular glaze calculation as a part of looking at glazes, it often helps to include the function of things like coloring oxides that act as fluxes or ampoterics into the main calculation....... but many people ignore this with everything except iron oxide.

 

best,

 

...............john

Share this post


Link to post
Share on other sites
Red Rocks    3

John and Mark:

 

Thanks for your responses, I checked with a few other people around here and their responses were very similiar, so next step will be to just mix up some small batches and test them. These are actually from my old glaze book at Arizona State, so they have not been mixed by me in a very long time.

Share this post


Link to post
Share on other sites

Create an account or sign in to comment

You need to be a member in order to leave a comment

Create an account

Sign up for a new account in our community. It's easy!

Register a new account

Sign in

Already have an account? Sign in here.

Sign In Now
Sign in to follow this  

×