MR. BUBBLES Posted July 24, 2012 Report Share Posted July 24, 2012 I'm wanting to fire some pendents and wind chimes which are heavier. I tried my 1/8 in stainless steel lampworking rods but they coulden't hold up to cone 6. What dose everyone use? Please help. Link to comment Share on other sites More sharing options...
Mark C. Posted July 24, 2012 Report Share Posted July 24, 2012 Heavy gauge Nichrome wire Support it as much as you can as well. Mark Link to comment Share on other sites More sharing options...
MR. BUBBLES Posted July 25, 2012 Author Report Share Posted July 25, 2012 Thanks, I'll check that out. Link to comment Share on other sites More sharing options...
Marcia Selsor Posted July 25, 2012 Report Share Posted July 25, 2012 Bead racks have sturdy nichrome rods. Would the pendants fit on those?Here is an example from Axner....the first supplier to pop up on Bing http://www.axner.com/bead-rack-small.aspx Marcia Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.