I'm looking for a cement grey speckled ^6 commercial glaze or a recipe to make such. Anyone know of anything?

Thanks
Bob.

#2 clay lover

clay lover

    Advanced Member

  • Members
  • PipPipPip
  • 1,150 posts
  • LocationSoutheast

Posted 01 July 2012 - 08:10 AM

I don't have a glaze suggestion for you, but I have used speckled clay (Highwater's speckled brownstone) and Opulence glaze-winter day to get a lovely speckled gray. Tucker also makes a good speckled whitestone that is good to work with. They both need to be bisques high enough to clean out the clay, I go to 1920*, could go some higher.