I'm applying clear matte glaze to portions of white, bisqued earthenware and I can't tell where I've put the glaze because they're the same color. If I color my glaze w/ food coloring, just so I can see where it is as I apply it, will that burn off in the kiln w/out affecting the glaze? Thanks.

#2 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,054 posts
  • LocationRaleigh, NC

Posted 19 June 2010 - 08:47 AM

I have used the red and it burns out ...don't know about the others.

Chris Campbell

Contemporary Fine Colored Porcelain
www.ccpottery.com

 

TRY ... FAIL ... LEARN ... REPEAT

" ... If a sufficient number of people are different, no one has to be normal"
Fredrick Bachman


#3 Icyone2

Icyone2

    Member

  • Members
  • PipPip
  • 18 posts

Posted 21 June 2010 - 12:49 PM

I've heard of people using food coloring in wax relief and it fires out

#4 Jacqui

Jacqui

    Newbie

  • Members
  • Pip
  • 3 posts
  • LocationCape Town, South Africa

Posted 22 June 2010 - 08:27 AM

I've heard of people using food coloring in wax relief and it fires out


I am not sure about this entirely, I would imagine it fires out. I did notice a whole lot of food colouring in my office when I recently took on a position as a ceramics technician, so I will get round to testing this out. although I would bet on them firing out completely .

#5 pent19

pent19

    Advanced Member

  • Members
  • PipPipPip
  • 37 posts

Posted 16 July 2010 - 09:21 PM

I have done this in my k-6 classroom to help distinguish glazes from each other (add red to clear, blue to blue-looks too much like green). I haven't noticed any problems, but then again, its on children's work and having residue is the least of my worries!

#6 Zygote

Zygote

    Member

  • Members
  • PipPip
  • 13 posts
  • LocationNorthern California

Posted 16 July 2010 - 11:44 PM

I know blue works. I use it for both wax and glazes

#7 JBaymore

JBaymore

    Moderator

  • Moderators
  • 4,119 posts
  • LocationWilton, NH USA

Posted 17 July 2010 - 08:32 AM

Most food coloring burns out....but not all. I have seen greens and blues that leave traces. Red and yellow usually are safe bets. But the real issue is to simply test the colors and brand you might use in a white glaze. Then you'll know for sure.

best,

.................john

John Baymore
Professor of Ceramics; New Hampshire Insitute of Art

Guest Professor, Wuxi Institute of Arts and Science, Yixing, China

Former President and Past President; Potters Council
 

http://www.JohnBaymore.com

http://www.nhia.edu/...ty/john-baymore





0 user(s) are reading this topic

0 members, 0 guests, 0 anonymous users