Posted 26 March 2012 - 02:18 PM

The only cobalt I have at home is in the oxide form. Most recipes that I see use the carbonate form. Is there a conversion so that I can substitute the oxide for the carbonate?

Bobg

#2 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,079 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 26 March 2012 - 09:47 PM

This was covered here

http://ceramicartsda...__fromsearch__1
Mark Cortright
www.liscomhillpottery.com

#3 Bobg

Bobg

    Advanced Member

  • Members
  • PipPipPip
  • 83 posts
  • Locationsoutheastern WA

Posted 29 March 2012 - 10:11 AM

Thanks Mark that's what I was looking for.