Bisques questions for electric kiln


  • Please log in to reply
4 replies to this topic

#1 confused_yet_curious

confused_yet_curious

    Advanced Member

  • Members
  • PipPipPip
  • 39 posts
  • LocationPhiladelphia

Posted 18 March 2012 - 05:15 PM

Hi everyone,
I'm doing an bisques in an baily's electric kiln. I did an pre heat for 5 hours ( had some dap pieces) and the pre heat started at 10 pm last night 03/17/12 so pre heat should of stopped at 3am today. I came In today at 10 am and the kiln was readiing 1022. Now I came in today at 5:30 pm and my kiln is reading 1179. That seems wrong to read to me, but I wanted to see what all of you felt! Thanks in advance!

#2 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,318 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 18 March 2012 - 06:39 PM

Hi everyone,
I'm doing an bisques in an baily's electric kiln. I did an pre heat for 5 hours ( had some dap pieces) and the pre heat started at 10 pm last night 03/17/12 so pre heat should of stopped at 3am today. I came In today at 10 am and the kiln was readiing 1022. Now I came in today at 5:30 pm and my kiln is reading 1179. That seems wrong to read to me, but I wanted to see what all of you felt! Thanks in advance!



I need more info-is that 1179 reading going up in temp or cooling down?????
If its going up then its way to slow-that fire should be way over by 5.30pm If its cooling then you are fine.
Mark


Mark Cortright
www.liscomhillpottery.com

#3 confused_yet_curious

confused_yet_curious

    Advanced Member

  • Members
  • PipPipPip
  • 39 posts
  • LocationPhiladelphia

Posted 18 March 2012 - 07:08 PM


Hi everyone,
I'm doing an bisques in an baily's electric kiln. I did an pre heat for 5 hours ( had some dap pieces) and the pre heat started at 10 pm last night 03/17/12 so pre heat should of stopped at 3am today. I came In today at 10 am and the kiln was readiing 1022. Now I came in today at 5:30 pm and my kiln is reading 1179. That seems wrong to read to me, but I wanted to see what all of you felt! Thanks in advance!



I need more info-is that 1179 reading going up in temp or cooling down?????
If its going up then its way to slow-that fire should be way over by 5.30pm If its cooling then you are fine.
Mark

Hey Its complete and now it's cooling down. This sort of delays me but I'm glade it's just cooling down. Have together them out and put my glazes on them. And have them ready by 4:30 this monday! Pray for me! Thank you for your help.

#4 Mark C.

Mark C.

    Advanced Member

  • Members
  • PipPipPip
  • 6,318 posts
  • LocationNear Arcata Ca-redwood rain forest

Posted 18 March 2012 - 07:25 PM

WAS THAT A COOLING TEMP??at 5.30pm
1179 or was it still heating up??
inquiring minds need to know?
Mark
Mark Cortright
www.liscomhillpottery.com

#5 confused_yet_curious

confused_yet_curious

    Advanced Member

  • Members
  • PipPipPip
  • 39 posts
  • LocationPhiladelphia

Posted 18 March 2012 - 07:26 PM

WAS THAT A COOLING TEMP??at 5.30pm
1179 or was it still heating up??
inquiring minds need to know?
Mark

It was the cooling down temp