I have a SHIMPO RK-10 GOLD wheel in like new condition I purchased years ago and then never really had a chance to use it. Build date is 1986 and it has a mettalic traction drive. Does anyone out there know weight capacity of clay it can handle? 

Thanks for any help!!

Johnita

Share this post


Link to post
Share on other sites

It's a 1/3rd hp, pulley drive, probably handle 50ish lbs.  I have an rk2 at 1/4 hp and the most Ive thrown is 30lbs, but it was just as fine as centering 10lbs as far as the wheel goes.