Jean Benoit Posted October 18, 2018 Report Share Posted October 18, 2018 I used colored slip on a white slip. Both fired to cone 04. I used a cone 04 clear glaze. The result: the white glaze is streaky, most of the colors have disappeared or altered. Why? Link to comment Share on other sites More sharing options...
liambesaw Posted October 18, 2018 Report Share Posted October 18, 2018 Is it a zinc free clear glaze? Also what percentage of stains did you use in your slip recipe Link to comment Share on other sites More sharing options...
Babs Posted October 19, 2018 Report Share Posted October 19, 2018 Are u putting a white glaze on top of coloured slip...a well yrs it will disappar most colours unless strong cobalt or other v strong colours How are you applying your white glaze ? Link to comment Share on other sites More sharing options...
Babs Posted October 19, 2018 Report Share Posted October 19, 2018 Sorry you used a clear glaze is it the glaze or slip which is streaky? Streaky showing underlying clay colour? Need to apply more coats of slip or a thicker slip. More colour product in your slips would intensify. Most colours pop under a clear glaze if it is not applied too thickly or overfired. Maybe run a few test pots Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.