Posted 13 January 2012 - 08:24 PM

I have a niece that is getting married in June. Years ago my Aunt made ceramic doves for the center pieces of mine and my sisters wedding tables. I wanted to make some for my nieces wedding. Two for each table. These doves are made of pinch pot halves put together and then wings and beaks. I put two holes in each that double as eyes and a place for the air to escape when I fire. They all have flat bottoms and are completely enclosed. I was wondering if I would ensure success a bit more if I carved out the bottom so they had a hole there as well. I have only done one pod style piece before and that was in a class. Any suggestions anyone could help me with? I'm worried I may have forgotten since my class was last year.
Thanks so much
Renee


Posted Image


#2 Chris Campbell

Chris Campbell

    clay stained since 1988

  • Members
  • PipPipPip
  • 3,064 posts
  • LocationRaleigh, NC

Posted 13 January 2012 - 08:44 PM

The two eye holes will be enough as long as the birds are 100%' ... No doubts ...dry.
Put them up to your face and if they feel cool they are not dry.
Another cute touch is to put dry clay pieces inside ... Shake to keep them loose and after firing you have a rattle.

Chris Campbell

Contemporary Fine Colored Porcelain
www.ccpottery.com

 

TRY ... FAIL ... LEARN ... REPEAT

" ... If a sufficient number of people are different, no one has to be normal"
Fredrick Bachman


#3 meisie

meisie

    Advanced Member

  • Members
  • PipPipPip
  • 105 posts
  • LocationMassachusetts

Posted 13 January 2012 - 08:51 PM

oh I like the rattle idea!!! I have learned my lesson on the absolutely dry part. So I want them made so they can sit a month or so before I fire. Thanks!


The two eye holes will be enough as long as the birds are 100%' ... No doubts ...dry.
Put them up to your face and if they feel cool they are not dry.
Another cute touch is to put dry clay pieces inside ... Shake to keep them loose and after firing you have a rattle.



#4 Growin' Granny

Growin' Granny

    Member

  • Members
  • PipPip
  • 12 posts
  • LocationShedd, Oregon and Borrego Springs, CA (snowbird)

Posted 14 January 2012 - 03:38 AM

oh I like the rattle idea!!! I have learned my lesson on the absolutely dry part. So I want them made so they can sit a month or so before I fire. Thanks!



The two eye holes will be enough as long as the birds are 100%' ... No doubts ...dry.
Put them up to your face and if they feel cool they are not dry.
Another cute touch is to put dry clay pieces inside ... Shake to keep them loose and after firing you have a rattle.



Sheila Maier


“A good traveler has no fixed plans and is not intent on arriving.” – Lao Tzu

#5 Growin' Granny

Growin' Granny

    Member

  • Members
  • PipPip
  • 12 posts
  • LocationShedd, Oregon and Borrego Springs, CA (snowbird)

Posted 14 January 2012 - 03:40 AM

You can also wrap the small clay pieces in a bit of paper towel or newspaper to keep them from sticking; then you don't have to remember to shake them while they're drying.

Sheila Maier


“A good traveler has no fixed plans and is not intent on arriving.” – Lao Tzu

#6 neilestrick

neilestrick

    Neil Estrick

  • Members
  • PipPipPip
  • 4,816 posts
  • LocationGrayslake, IL

Posted 14 January 2012 - 09:44 AM

Don't worry about air holes. The eye holes are more than enough. You can fire pieces that are completely sealed. We do it all the time at my shop. Expanding air does not blow up pots. Air bubbles do no blow up pots. Steam blows up pots. You just have to make sure the pieces are completely dry, which means letting them dry much longer than normal. Because they are sealed up, they can appear dry on the outside while still being wet on the inside. It's not a bad idea to do a preheat in the kiln.

Neil Estrick
Kiln Repair Tech
L&L Kilns Distributor
Owner, Neil Estrick Gallery, LLC
www.neilestrickgallery.com

neil@neilestrickgallery.com


#7 OffCenter

OffCenter

    Advanced Member

  • Members
  • PipPipPip
  • 1,372 posts

Posted 14 January 2012 - 11:09 AM

Don't worry about air holes. The eye holes are more than enough. You can fire pieces that are completely sealed. We do it all the time at my shop. Expanding air does not blow up pots. Air bubbles do no blow up pots. Steam blows up pots. You just have to make sure the pieces are completely dry, which means letting them dry much longer than normal. Because they are sealed up, they can appear dry on the outside while still being wet on the inside. It's not a bad idea to do a preheat in the kiln.


Thanks, Neilestrick, for posting that. It is amazing how many experienced potters still think that air pockets and trapped air blow pots up!

Jim
E pur si muove.

"But it does move," said Galileo under his breath.

#8 meisie

meisie

    Advanced Member

  • Members
  • PipPipPip
  • 105 posts
  • LocationMassachusetts

Posted 14 January 2012 - 05:39 PM

Interesting. I did have one firing where I lost quite a few pot largely due to each having a heavy base and not being dry enough. I won't make that mistake again. regardless I think with these I am going to do a preheat because you're right it's hard to tell how dry they are going to be on the inside.

Don't worry about air holes. The eye holes are more than enough. You can fire pieces that are completely sealed. We do it all the time at my shop. Expanding air does not blow up pots. Air bubbles do no blow up pots. Steam blows up pots. You just have to make sure the pieces are completely dry, which means letting them dry much longer than normal. Because they are sealed up, they can appear dry on the outside while still being wet on the inside. It's not a bad idea to do a preheat in the kiln.