docweathers Posted December 1, 2016 Report Share Posted December 1, 2016 Has anyone used Bringle Universal Slip? Neph Sy 25 Kaolin 20 Ball 20 Flint 30 Borax 5 Bentonite 2 What have you found it good for? Does it run at cone 6? Does it work for mocha diffusion? Is supposed to fire from: 1 to 6 That seems like a real stretch to me. Link to comment Share on other sites More sharing options...
bciskepottery Posted December 2, 2016 Report Share Posted December 2, 2016 I use Bringle slips at cone 10 for salt and wood firing. Can be applied at either greenware or bisque stages, although thinner at bisque. Have not tried at cone 6. Link to comment Share on other sites More sharing options...
docweathers Posted December 2, 2016 Author Report Share Posted December 2, 2016 You say slips plural. Are you using the formula that I posted? Link to comment Share on other sites More sharing options...
bciskepottery Posted December 2, 2016 Report Share Posted December 2, 2016 bringleslip.pdf You've listed the base slip recipe. Then you get to add oxides and colorants for variations. Link to comment Share on other sites More sharing options...
docweathers Posted December 2, 2016 Author Report Share Posted December 2, 2016 Okay I got it. The plural was referring to different colors versus different base Slips. It's pretty amazing stuff if it actually works from ^1 to ^10 Thanks Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.