docweathers Posted October 24, 2016 Report Share Posted October 24, 2016 I'm applying glaze to bisque. It starts to crack as soon as the shine is gone. Shortly large flakes are falling off of vertical surfaces. Lalone Crawl is one of the worst., It is very high in magnesium. But I don't want to reduce the magnesium because I like the fired affect very much. Nepheline Syenite 70 Ball Clay 5 Magnesium Carbonate 25 I would appreciate any suggestions on how I can get the glaze to stick. thanks Link to comment Share on other sites More sharing options...
terrim8 Posted October 25, 2016 Report Share Posted October 25, 2016 try putting a thin layer of slip beneath the glaze? I've tried this with beaded glaze and it works most of the time. Link to comment Share on other sites More sharing options...
docweathers Posted October 25, 2016 Author Report Share Posted October 25, 2016 That's a good idea. I will give it a try. Link to comment Share on other sites More sharing options...