jmpeden Posted June 14, 2016 Report Share Posted June 14, 2016 Im having trouble with spectrum satin speckle blistering. I use Laguna clay that is bisqued to 04. Im firing in an L & L electric kiln at slow glaze to cone 6. I also tried coyote creamy matte at the same temp and it also had some blistering. I did apply kinda thick so could that be part of the problem? Link to comment Share on other sites More sharing options...
neilestrick Posted June 14, 2016 Report Share Posted June 14, 2016 Thickness could be an issue. I would also try firing to 5 instead of 6. It could be that your kiln is not calibrated properly, so it's firing a bit hot. Have you put cones in to verify the heat work? Link to comment Share on other sites More sharing options...
jmpeden Posted June 14, 2016 Author Report Share Posted June 14, 2016 No i havent put cones in. Link to comment Share on other sites More sharing options...
Roberta12 Posted June 15, 2016 Report Share Posted June 15, 2016 Specifically, which Laguna clay is it? Roberta Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.