I am new to the digital controller on my kiln (Sentry 2.0 controller) and would really appreciate some help in programming a cone 5 firing with a 1 h. preheat and a slow cool. Does this make sense?

 

rA1 = 60, F1 = 200, Hd = 1  (preheat with 1 hr. hold at 200 degrees)

rA2 = 200, F1 = 1022, Hd = 0

rA3 = 153, F1 = 1112, Hd = 0

rA4 = 162, F1 = 1951, Hd = 0

rA5 = 108, F1 = 2167, Hd = 0

rA6 = 500, F1 = 1900, Hd = 0  (begin slow cool)

rA7 = 125, F1 = 1450, Hd = 0

rA8 = 0

 

Can I assume after rA7 it will cool naturally?

rA2 - rA5 are what my Sentry manual says it uses to reach cone 5.

 

I am really happy this forum is here - I have learned so much from you all!

 

Thank You

Dianne

Link to comment
Share on other sites

Dianne-

Curious as to why you are using a preheat with a hold. Are you firing greenware with glaze, or are you firing immediately after glazing? If glaze firing bisque, there really isn't a need for such a slow preheat and hold below the boiling point of the physical water.

Link to comment
Share on other sites

Archived

This topic is now archived and is closed to further replies.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.