When you say check it with cones,I think I did that. The cones in for the first firing with this new TC were one 5,the firing schedule I use normally gives me cone six. I need to run a glaze load tomorrow morning. I'm guessing and adding 10* to the peak temp with the same firing rate. I've got cones in, we will see. The 1/2 cone cooler left several of my glazes blah.