jrgpots Posted September 28, 2015 Report Share Posted September 28, 2015 I have some Laguna dynasty red cone 6 glaze. It is a it bland. I have been thinking of adding rutile to give some interest. Has anyone used or tweeked this glaze with success? Jed Link to comment Share on other sites More sharing options...
GiselleNo5 Posted September 28, 2015 Report Share Posted September 28, 2015 I use Dynasty Red. I always do four coats to get thick even color. I haven't experimented with mixing different ingredients but I have done some layering with it. My favorite combination was with Laguna's Antique Jade over it. Very pretty. Link to comment Share on other sites More sharing options...
jrgpots Posted September 28, 2015 Author Report Share Posted September 28, 2015 Can you post a pic of it? Jed Link to comment Share on other sites More sharing options...
GiselleNo5 Posted September 28, 2015 Report Share Posted September 28, 2015 I will tomorrow. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.