Made a slip from my new clay formula and cast my 12 x16 arched tile mold yesterday. Popped it out of the mold and hour later and it is still perfectly flat this afternoon. First time that has happened.
Joseph Fireborn
Congrats, your hard work paying off mate.
glazenerd
Joseph: so far all I have to do is roll and cut. I do not touch them again until they are bone dry. No turning or weighting- cuts labor way down.
Marcia Selsor
looks like you may be onto something!