Hi there, no I don't mind input about Numerology, I find it all quite interesting, so if you have any other information, I would be most intrigued. About your cracked bottoms on your pots. I have a feeling this is due to too much use of water when joining. When I work with slabs, and score my slabs on both surface areas I then use a slip , which I make up as a paste from the clay I'm wo...