Jump to content

WildCelticRose

Members
  • Content count

    45
  • Joined

  • Last visited

About WildCelticRose

  • Rank
    Member
  • Birthday 10/24/1962

Contact Methods

  • Website URL
    http://wildcelticrose.net

Profile Information

  • Gender
    Female
  • Location
    Tacoma, WA
  • Interests
    realizing my dream (since Jr High School) of having my own ceramics studio)

    Always in awe of how fire transforms minerals and earth into glass, and art...

    Kind of a metaphor for life, don't you think?
  1. OOooh! So many great ideas and links. I actually like the idea of some of the crayons leaving some pigment, I can use that for some shading inside. On some of the larger designs on the white clay, it's too much white. When I'm doing runs of 200+ pieces, liquid anything is just too much to deal with, especially if it's waxy gets where it shouldn't. Please keep the ideas coming. As far as stamping, for the larger bits, I'm thinking about creating tiles and rolling the outside of the cup for bowl on the tile to create the impression.
  2. Hi folks. I've been using a Silhouette Cameo cutter to create vinyl decals I put on my bisque before dipping in glaze to create a negative space design. (it's ain't easy creating a signature look and standing out in an art town) It's challenging (sometimes flat crazy making) because if you pull the decals too soon, glaze runs into the area you want to keep clean and too late, it flakes and chunks come off with the decal and I end up doing a lot of clean up or touch up. Add to that my unnatural love of gooey, reactive, unpredictable and persnickety glazes and it can be a real PITA, especially when doing runs of 200+ pieces. My cutter just broke and I won't be able to afford a new one any time soon. Once I was done stressing out and having a mini meltdown, I decided to try to create something new, different and cooler. I was thinking about carving stamps of my more popular designs and then using crayons as wax resist (I have no love for liquid wax resist and a very complicated history with it) Crayons are crazy cheap at the dollar store and easy to control. Bonus, I can leave some small bits unwaxed to add shadow/more texture... I've only made one stamp, I carved into some craft plaster of paris advertised as “carvableâ€, then pushed wet clay into the carving and bisque fired to create a stamp. So here are my questions…. Has anyone ever used crayons as wax resist? And did they work well for you? What is your favorite carving material for making stamps? I've added a couple of photos of what I've been doing to provide a visual… Thanks in advance
  3. Firing Disaster? Fired For 20 Hours - 9 Hour Soak?

    exhausted, sleep deprived, stressed out, menopausal (back off or I will cut you) human error
  4. Firing Disaster? Fired For 20 Hours - 9 Hour Soak?

    Neil, That's what I was thinking... It's what I'm hoping. It's a fairly new kiln with a Sentry 2.0 controller and I was extremely perplexed that there was no error message. The one time the kiln didn't reach temperature in time (an early firing before I had the hang of it) it shut off and gave me an error code. Between the day job and the project from hell I was pulling 18 hour days (sometimes more) and I was crazy exhausted and stressed out on that last firing (and I had already screwed up a ramp and hold on a bisque firing which is why things went explody and put me behind schedule. Tonight I'm going to run my regular cone 5 program with a five minute hold (my plum red glaze needs that to not look quite so purple) with shelves and cones and see what happens. I'm really hoping it was me, not the kiln because I need to get back at it as I have a backlog of work. Marc, I agree with the sleeping thing. While less than ideal, it's how things are sometimes. My kiln is properly installed and wired to specs on its own circuit. I was with my electrician friend when he installed it and it was done with extra electrical safety in mind. It is on a metal stand on a concrete floor and the walls are concrete. There are no combustibles anywhere near it. I set it to finish firing just before I wake up for work so I am there if something goes wrong and it doesn't shut off.... THAT was my error this time. It was within a few degrees of shutting down and I didn't want to be late for work. I won't be doing that again. While nothing is ever 100% safe, the lint trap in my dryer is a greater fire hazard as is my gas water heater which has a pilot light. I really do want to thank everyone who has chimed in on this post. It's nice to know that there's a community out there how had my back on this
  5. Firing Disaster? Fired For 20 Hours - 9 Hour Soak?

    by 'you guys" if you mean me, yes. I have a full time day job which means I can't be awake during all cycles of firing.
  6. Firing Disaster? Fired For 20 Hours - 9 Hour Soak?

    I ran a test fire to cone 5 last night on the fast setting. It wasn't quite done when I went to bed. When I woke up this morning, it had taken 8:45 which is about right. Next, I'll run a test on a regular fire with a 5 minute hold with shelves and cones to see what the cones do. I may be OK.
  7. Firing Disaster? Fired For 20 Hours - 9 Hour Soak?

    That's why I pulled the cover and visually inspected both relays and all the wiring, someone here locally has had the singed relay thing happen to them as well. Of course... I unplugged my kiln first... Jussayin'
  8. Firing Disaster? Fired For 20 Hours - 9 Hour Soak?

    Ugh! How did you find out that it switched off at 600 degrees?
  9. Firing Disaster? Fired For 20 Hours - 9 Hour Soak?

    Sometimes it pays to go low tech... both relays work and the middle elements aren't burned out or broken. All I can do now is run a test fire to see if my maintenance and reset work and/or if the misfire was a fluke or a programming error... If the test fire doesn't complete or takes too long, I'll need to go buy an ohm meter for further testing. In any event, I've become very well acquainted with my kiln's guts.
  10. Firing Disaster? Fired For 20 Hours - 9 Hour Soak?

    Mark, THANK YOU! I went through my kiln manual and the center elements are variable. I felt around and nothing seems broken, although I did find some exploded bits of pottery here and there. I pulled the cover off my controller to check for any shorted out wiring (at the suggestion of a local potter and mentor) and it all looks good. I'm going to give the kiln a good vacumming and then try the "newspaper" test to see if they are getting hot; after all, they only need to get to 451 degrees...
  11. Firing Disaster? Fired For 20 Hours - 9 Hour Soak?

    I finally got around to testing the kiln today. I needed about two weeks of sleep after that adventure and also had a CD/book release as well as insanity at work. I did a quick fire to 1,000 degrees. As I suspected, the middle elements weren't red. I aborted the program (no sense paying the electric charge for a full firing) and unplugged it. Tomorrow when it's cool I'll inspect the elements. That is the area where the shelf that collapsed hit and broke brick so that is the most likely scenario. (and I'm hoping the most easy to fix) If not, I'll have to look at wiring in the controller box and that relay. Thanks again everyone for all your support and for caring.
  12. Firing Disaster? Fired For 20 Hours - 9 Hour Soak?

    Mmmm. I think I'll pass on that ten hour hold one. Those make me twitch
  13. Firing Disaster? Fired For 20 Hours - 9 Hour Soak?

    I mean who knows.. It's a computer, it might be as simple as...
  14. Firing Disaster? Fired For 20 Hours - 9 Hour Soak?

    It was showing the temp like it was climbing, it would read 2111, then 2112, then 2111, etc.... I was tempted to start the fire again so the cool down would be slower in the critical phases, but a quick call to my mentor confirmed that since everything was likely badly overfired, it would be smarter to just abort the program and leave it to cool which I did.
  15. Firing Disaster? Fired For 20 Hours - 9 Hour Soak?

    That is a very interesting theory. I was so exhausted when I was programming and didn't want to make a mistake and ran through it multiple times, so that is a possibility. I'm hoping to have the time to give it a good going over at some point over the weekend to rule out anything physical.
×