This bowl was a bit of a surprise. The interior is suposed to be chartreuse! Luckly the steel blue color is beautiful!

 

Black Mountain Clay with 3 coats of white Amaco Velvet Undeglaze, followed by 3 coats of chartreuse Amaco Velvet Underglaze before bisque firing. Then 3 coats of Amaco's zinc free clear fired to ^10. I also antiqued the outside with a cobalt oxide wash (which turns blue-black on the black mountain clay) to accent the texture.

 

The texture was carved into thick walls while the clay was leather hard.


Copyright

© Aug 2014
Sign in to follow this  
From the album:

Texture

  • 2 images
  • 0 comments
  • 1 image comment

Photo Information for Textured Bowl 1 - Final

Taken with Apple iPhone 5

  • 4.1 mm
  • 1/143
  • f f/2.4
  • ISO 50
View all photo EXIF information

Recommended Comments

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.