Stoneware, wood fired and electric fired. Ice Crackle glaze. Luster. In private collection in South Korea.

Copyright

© &copy John Baymore all rights reserved
Sign in to follow this  
From the album:

John Baymore's Clay Work

  • 31 images
  • 0 comments
  • 38 image comments


Recommended Comments

Beautiful crackle glaze, John. The glaze color and earthy contrast of the transition of the edge where the glaze is thin and breaking over reminds me of a slab of chalcedony that I had had for many years. Stunning!

 

- rick

Share this comment


Link to comment

Thanks AmeriSwede and Sylvia.

 

Sylvia....... if you are talking about applying over stoneware clay bodies at about Orton cone 9-10, ge the C.O.E. of your feldspathic glaze up to about 8 and you'll be happy.

 

 

best,

 

..............john

Share this comment


Link to comment

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Add a comment...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.