Poplar Ridge Posted February 12, 2011 Report Share Posted February 12, 2011 OOPS!! I left a bucket of wet scraps outside and forgot about it. Needless to say it froze. Can the clay be used after wedging like I regularly do, or does it make any difference that it was frozen? Link to comment Share on other sites More sharing options...
Seasoned Warrior Posted February 12, 2011 Report Share Posted February 12, 2011 OOPS!! I left a bucket of wet scraps outside and forgot about it. Needless to say it froze. Can the clay be used after wedging like I regularly do, or does it make any difference that it was frozen? I doubt freezing would make any difference, after all clay in nature freezes and thaws many cycles, in fact that is part of how it becomes clay. Regards, Charles Link to comment Share on other sites More sharing options...