Ginny C Posted January 28, 2015 Report Share Posted January 28, 2015 Haven't used this terra sig in a long time, so it's pretty solid now in the bottom of the container. I need just a little for some pot feet. Can I add water and stir? Or add some other liquid? Or is it hopeless? Thanks for a quick reply. I'm working on some lovely bowls and want silky smooth feet on them. Ginny Clark Link to comment Share on other sites More sharing options...
TJR Posted January 28, 2015 Report Share Posted January 28, 2015 Sure. Add water. TJR. Link to comment Share on other sites More sharing options...
Marcia Selsor Posted January 29, 2015 Report Share Posted January 29, 2015 Yes but don't over water. Marcia Link to comment Share on other sites More sharing options...