TortoiseAvenger Posted July 16, 2014 Report Share Posted July 16, 2014 Anyone work with this? I'm getting into sculpture and it seems pretty cool. I just finished making a batch. The biggest benefit I see touted is the ability to connect bone dry pieces. Are there other benefits? Anything I should know before I start? I can still single fire with it I assume. (I know about the smoke it creates.) Any tips or info would be helpful. Thanks! Link to comment Share on other sites More sharing options...
Marcia Selsor Posted July 16, 2014 Report Share Posted July 16, 2014 I have used it, Usually add a small handful to 200 pound batch of dry clay. Dissolve it first in water for better mixing. I prefer paper clay to adding nylon. I think it is more versatile.And you can add greenware to bisque. Marcia Link to comment Share on other sites More sharing options...