Boats Posted May 12, 2014 Report Share Posted May 12, 2014 Does anyone have any ideas on how to replicate Mayco's Midnight Rain. I would like to experiment with variations; however, I am really in the dark as to where to start to obtain this kind of effect. I find the interaction of the blues and greens along with the running oil spot effect intriguing. I would greatly appreciate ideas on where to start with a basic recipe. Link to comment Share on other sites More sharing options...
williamt Posted May 12, 2014 Report Share Posted May 12, 2014 The base looks like a cone 6 float blue recipe (several on the net). The Mayco catalog says there are quartz chunks that melt for the oil spots, could be an iron or manganese course frit? Lee Link to comment Share on other sites More sharing options...
Boats Posted May 13, 2014 Author Report Share Posted May 13, 2014 Thanks Lee, I'll play with that combination and see what happens. Link to comment Share on other sites More sharing options...
williamt Posted May 13, 2014 Report Share Posted May 13, 2014 Good luck! Let me know what you get. Link to comment Share on other sites More sharing options...
Recommended Posts
Archived
This topic is now archived and is closed to further replies.