grajewski Posted February 20, 2014 Report Share Posted February 20, 2014 Hi, I would like to get a typical french glaze recipy, green and yellow, appr. 1020-1080 celcius have seen lots in France but never seen how to make the glaze. Thanks ! Link to comment Share on other sites More sharing options...
Marcia Selsor Posted February 20, 2014 Report Share Posted February 20, 2014 I think you are referring to French Faience most notably from the Quimper pottery. This link explains the process for Faience also known as Majolica. http://ceramicartsdaily.org/ceramic-glaze-recipes/low-fire-glaze-recipes/messing-with-majolica-an-instructor-shares-tips-for-learning-and-teaching-the-majolica-technique/ I hope this is what you meant. Marcia Link to comment Share on other sites More sharing options...