Hello,

Is it possible to use wadding on a bisque firing of cone 04 and then wadding on the glaze firing cone 5 or 6 on a hollow porcelain piece that has a small pour hole opening? Can you us wadding with porcelain?  Does the wadding just come off the piece?  Thank you!  I appreciate  all the help that any one can give me!!! Sandi

Edited by Sandi0720
Link to comment
Share on other sites

18 hours ago, Sandi0720 said:

Hello,

Is it possible to use wadding on a bisque firing of cone 04. Can you us wadding with porcelain?  Thank you,  Sandi

Thanks for asking this @Sandi0720  I have wondered the same thing myself.  I have some small dishes I make for a local pet store.  The stilts work fine for that.  But I have wondered about using wadding for bisque and glaze firing on porcelain!  

 

Link to comment
Share on other sites

Join the conversation

You can post now and register later. If you have an account, sign in now to post with your account.

Guest
Reply to this topic...

×   Pasted as rich text.   Paste as plain text instead

  Only 75 emoji are allowed.

×   Your link has been automatically embedded.   Display as a link instead

×   Your previous content has been restored.   Clear editor

×   You cannot paste images directly. Upload or insert images from URL.

×
×
  • Create New...

Important Information

By using this site, you agree to our Terms of Use.