Yvonne badoni Posted January 14 Report Share Posted January 14 I just got a new bottle of hot tamale stroke and coat. Seems to have tiny crystals in it? Will it still work? Quote Link to comment Share on other sites More sharing options...
neilestrick Posted January 14 Report Share Posted January 14 1 hour ago, Yvonne badoni said: I just got a new bottle of hot tamale stroke and coat. Seems to have tiny crystals in it? Will it still work? Hi Yvonne, welcome to the forum. Can you post a picture of the crystals? Are they flat flakes or round bits? As far as I can tell this isn't a product that should have crystals in it like some glazes do. As to whether or not it'll still work, that would require testing unless someone else speaks up with the same experience with that glaze. Quote Link to comment Share on other sites More sharing options...
Yvonne badoni Posted January 14 Author Report Share Posted January 14 They are very tiny roundish crystals. Maybe it has been frozen or something? Quote Link to comment Share on other sites More sharing options...
PeterH Posted January 14 Report Share Posted January 14 Perhaps relevant. Flambe magic John Britt investigates the appearance of mysterious crystals in the glaze slop. http://ceramicstoday.glazy.org/articles/flambe_magic.html Quote Link to comment Share on other sites More sharing options...
Recommended Posts
Join the conversation
You can post now and register later. If you have an account, sign in now to post with your account.