Ginny C Posted October 3, 2023 Report Share Posted October 3, 2023 I have an Excel 700 Select Fire kiln. Started it on slow cone 5 and later wished I had chosen medium speed...or maybe slow cool. Just curious, is it harmful to stop the firing part way through and restart it in another program? Quote Link to comment Share on other sites More sharing options...
Bill Kielb Posted October 3, 2023 Report Share Posted October 3, 2023 (edited) In my experience Likely no worries as long as the controller will resume the new program. Until you get within the last 200 - 300f degrees of your cone in theory not much of the final melting work has been done so everything should be fairly reversible. Edited October 3, 2023 by Bill Kielb Callie Beller Diesel 1 Quote Link to comment Share on other sites More sharing options...