jwt Posted October 1, 2023 Report Share Posted October 1, 2023 twice have not been able to reach temperature. Firing propane, replaced the regulator but still couldn't get up to temp, not even cone 4. The weather was warm and humid,88. The burners are older, could they need to be cleaned (sand blasted)? I am at a bit of a loss. Any ideas? Thanks Quote Link to comment Share on other sites More sharing options...