twice have not been able to reach temperature. Firing propane, replaced the regulator but still couldn't get up to temp, not even cone 4. The weather was warm and humid,88. The burners are older, could they need to be cleaned (sand blasted)? I am at a bit of a loss. Any ideas?
Thanks