SailorSoane Posted June 2, 2023 Report Share Posted June 2, 2023 Hi all, I'm new to making my own glazes. I'm wondering if anyone knows if the Shimpo ball mills will work for granite? I have a lot of granite on my property and would like to grind some up for testing. Many thanks in advance. Quote Link to comment Share on other sites More sharing options...
Min Posted June 2, 2023 Report Share Posted June 2, 2023 Hi and welcome to the forum! Old thread here discussing ball milling granite, some calcine the granite first and some don't. https://community.ceramicartsdaily.org/topic/6750-tumbler-ball-mill/ Quote Link to comment Share on other sites More sharing options...