LadyLumpsClay Posted October 21, 2022 Report Share Posted October 21, 2022 My thermocouple casing cracked after the fifth or sixth firing. Is it still okay to use or do I need to replace it already? Thank you! Quote Link to comment Share on other sites More sharing options...
neilestrick Posted October 21, 2022 Report Share Posted October 21, 2022 What type of thermocouple? Does it have a metal sheath, or do you mean the ceramic beads, or a protection tube? Post a pic. Quote Link to comment Share on other sites More sharing options...