Goyo Posted July 3, 2022 Report Share Posted July 3, 2022 We acquired a vintage (I assume) due to the controls and the construction. The sitter only has Low, Medium and high settings. Quote Link to comment Share on other sites More sharing options...
neilestrick Posted July 4, 2022 Report Share Posted July 4, 2022 The Sitter is just the shutoff device. The kiln itself has low-med-hi settings. Pretty much all kilns used Sitters for a few decades. All kilns of all brands with that control configuration work the same, and a typical firing schedule is 1 hour on low, 1 hour on medium, 1 hour on high. You can download a Sitter manual by Googling it. Quote Link to comment Share on other sites More sharing options...