CarinC Posted April 27, 2022 Report Share Posted April 27, 2022 hi all! I have a LL kiln model LT-3 model number J18x that I have inherited in our art room. I have only used a digital interface before. Can anyone provide some insight on using this? thanks! Link to comment Share on other sites More sharing options...
neilestrick Posted April 27, 2022 Report Share Posted April 27, 2022 HERE is a manual for the Kiln Sitter. A typical firing schedule would be 1 hour on low, 1 hour on medium, then high till the Sitter shuts it off. if you need to dry work, set the bottom section on low for a few hours with the lid cracked. Link to comment Share on other sites More sharing options...