JACKIE_O Posted February 24, 2022 Report Share Posted February 24, 2022 I accidentally fire done mica pots meant for cooking at 04. The look great and shiny. Can they still be used for stovetop cooking? Thank you Link to comment Share on other sites More sharing options...
Harold Roberts Posted March 2, 2022 Report Share Posted March 2, 2022 I have used micaceous clay from Santa Fe clay and I think that I fired it to cone 09. I have cooked in it many times but I think a lower temperature would be better. Since you have already fired it I think you have no choice but to try it out. Try boiling water in one. Some of mine have developed small cracks and leaked a little for awhile but have stopped after more use. Link to comment Share on other sites More sharing options...