LJackson10 Posted August 27, 2021 Report Share Posted August 27, 2021 I’m making decals with words on them and I was wondering if I should mirror the image so the words come out not backwards Link to comment Share on other sites More sharing options...
Callie Beller Diesel Posted August 27, 2021 Report Share Posted August 27, 2021 It depends if you’re making water slide or tissue transfer style decals. If you’re making water slide ones, no. If you are making them with silk screen or similar methods, you’ll have to reverse them. Link to comment Share on other sites More sharing options...