Katie Preece Posted August 24, 2021 Report Share Posted August 24, 2021 Hello Ive recently upgraded my kiln so no have 2 different size kiln shelves 350mm and 420mm, would it be okay to use them both in the same kiln load? Largest at the bottom. If so what's the best way to arrange the kiln probs? Many thanks Katie Link to comment Share on other sites More sharing options...
neilestrick Posted August 24, 2021 Report Share Posted August 24, 2021 You can use shelves that are smaller than the intended size, however you have to make sure that the posts still line up vertically. So move your posts at the bottom inward so they match up with the smaller upper shelves. It won't be the best use of the kiln space to use smaller shelves, but you can let the rims of bowls hang over the edges to fill some of the wasted space. Just don't let the foot hang over the edge. Link to comment Share on other sites More sharing options...