glenn Posted July 17, 2021 Report Share Posted July 17, 2021 i would like to create figures approx 10" to 12" tall - realistic. is it possible to keep them solid? it would be nearly impossible to hollow them out evenly unless there is a technique i an unfamiliar with. any recommendations would be greatly appreciated. much thanks glenn Link to comment Share on other sites More sharing options...
Chilly Posted July 17, 2021 Report Share Posted July 17, 2021 So long as no part is thicker than 12 - 15mm, and you let it dry thoroughly, and do a slow bisque, it could be ok. Pottery explodes when the inside of the form cannot dry, as it can't evaporate through the too-thick clay. You could cut a finished figurine in half, scoop out the inside, and rejoin. Or you could use your figurine as a master and make a plaster mould and cast the final object. Link to comment Share on other sites More sharing options...