Kelly in AK Posted November 15, 2022 Report Share Posted November 15, 2022 Hey @Pir, I usually seive twice because I'm obsessed with getting things well mixed, it's overkill except with certain materials (wollastonite and tin are chunky, cobalt oxide has to be well dispersed, things like that). I've read that Epsom salts need clay in the glaze to do it's trick, your recipe has plenty of clay though. I would not have expected that. Quote Link to comment Share on other sites More sharing options...