Alexia Merces Vidal Posted October 31, 2020 Report Share Posted October 31, 2020 Hello!! Can anyone tell me how can I do this glaze effect? Link to comment Share on other sites More sharing options...
neilestrick Posted October 31, 2020 Report Share Posted October 31, 2020 Looks to me like a single glaze that has been poured onto the piece to create areas of thicker and thinner application. You just need a glaze that varies in color due to thickness, which shouldn't be too hard to find. Link to comment Share on other sites More sharing options...